Formation of Hgcdte (McT) by Electrochemical Atomic Layer Deposition

HgCdTe or Mer-Cad-Tel is the most widely used Infrared material. The present study describes the growth of MCT via Electrochemical ALD, using an automated electrochemical flow cell deposition system.... This description may be from another edition of this product.